Biomimetic Structured Porogen Freeform Fabrication System for Tissue Engineering
71
Tensile test of 90/10 dogbone specimen-0.200.20.40.60.811.21.41.61.80 0.002 0.004 0.006 0.008 0.01 0.012 0.014 0.016 0.018 0.02
StrainStress (MPa)Fig. 13. Tensile stress-strain curve for a 90/10 PCL-CaP dogbone specimen.
Comparision of TM for Raw Materials020406080100120140160100 90 80
Percentage of PCLTM (Mpa)Comparision of UT S for Raw M aterials00.511.522.533.5100 90 80
Percentage of PCLUTS (Mpa)Fig. 14. Tensile mechanical properties of PCL-CaP composites (n6). A: Comparison of the
tensile modulus of 100% PCL, 90:10 and 80:20 PCL-CaP scaffolds; B: Comparison of the
ultimate tensile strength with different concentrations of CaP.